Fact Sheet
The DuPont Oval Logo, DuPont?, and Teflon? are trademarks or
registered trademarks of E.I. du Pont de Nemours and Company.
Use of DuPont trademarks subject to License Agreement and
qualification.
Description
Teflon? FEP topcoats provide nonstick, chemical and
corrosion resistance. Because FEP can melt-flow to
form nonporous film, it is a natural choice for release
applications with low abrasion such as molds and
bakeware.
The 856-line of Teflon? topcoats must be used with a
Teflon? industrial coatings primer. Examples:
FDA Conforming Not FDA
Primers Conforming Primers
858-100 851-204
959-200 series 850-300 series
959-405 958-200 series
FDA Status
The 856-200 Teflon? topcoat complies with FDA regulations
in 21CFR governing components of coatings
for direct food contact when applied according to fact
sheet instructions. Primers must also comply for the
system to be FDA conforming. Note: 856-204 and
856-211 Teflon? topcoats do not comply with FDA
regulations in 21CFR.
Table 1
Typical Properties
856-200 856-204 856-211
Color Clear Green Gray
% Weight Solids 44.9 44.1 46.3
% Volume Solids 26.4 24.4 24.3
Coverage, ft2/gal* 423 391 453
(m2/l)* 10.4 9.7 11.1
Viscosity, cP 20–400 50–300 20–300
Maximum use
temperature, °C (°F) 204 (400)
* Theoretical coverage at 25 μm (1 mil) assuming 100%
spray efficiency.
These figures are averages and may vary.
856-200, 856-204, and 856-211
DuPont? Teflon ? 856-Line FEP Topcoats
Application
Bring coating to room temperature. Roll or agitate
gently but thoroughly until contents are homogeneous.
Do not use a lightening mixer or similar type of mixer.
Strain through 100-mesh stainless steel screen.
See “Applying Teflon? Coatings” fact sheet.
Surface Preparation
Apply primer over clean and roughened surface and
apply as directed on primer fact sheet. Bake or force
dry per directions in appropriate primer fact sheet.
Film Thickness
Apply 856-2XX coatings at a total DFT of 15-25 μm
(0.6-1.0 mil) with a primer thickness of approximately
7 μm (0.3 mil). Flash dry to prevent popping or cracking
during the bake.
Bake
All temperatures refer to metal temperature. For end
uses where low porosity is essential, multiple topcoats
are required using the higher temperature bakes.
Primer
See specific fact sheets for primers.
Single top coat
The first topcoat must be sufficiently baked to cure the
primer. For example:
Bake If Using Primer
5 min. at 400°C (750°F) or 850-3XX line;
10 min. at 370°C (700°F) 851-204; 858-100
60 min. at 300°C (575°F) or 958-2XX line; 959-line